Borax_Method_of_Gold Recoverymercury_kidThe Gravity-Borax Method GBM is still unknown  to most Artisanal and small-scale gold miners (ASGMs) worldwide as most still use mercury to extract gold. “Whole-ore amalgamation” is a technique that requires the use of 10–25 g of mercury to produce 1 g of gold. Within the last eight years, it has become evident that this technique is more widely used than earlier anticipated, and artisanal small-scale gold mining (ASGM) is now considered the single largest contributor to global mercury pollution with the environmental release of 2,000,000 lbs of mercury per year. The United Nations Environment Programme has estimated that ASGM contributes a 37% share of the anthropogenic emission of mercury to the atmosphere.

Whole-ore amalgamation is commonly practiced in the Philippines. The ore is mixed with water and crushed in a rod mill (a rotating drum with metal rods inside), after which mercury is added and milled with the ore. The gold dissolves in the mercury and forms amalgam. After the milling, the content is poured into a tub where the mercury (holding the gold) sinks to the bottom. Excess mercury is recovered, and by blowtorching the remaining bit of amalgam, the mercury evaporates leaving behind the gold.

Leach Gold Without Cyanide

boaxIn Benguet province, a group of miners has been using the mercury-free gravity-borax method (GBM) for gold extraction for decades. This method basically requires the same equipment as the amalgamation methods. However, after the rod milling, an ore concentrate holding the heavy minerals is produced by using a launder (gold sluice) or a gold trommel. The heavy mineral concentrate is mixed with borax powder. By blowtorching the mix, the borax melts and the gold sinks to the bottom. It has recently been demonstrated that under identical conditions, GBM yields more gold than the traditional amalgamation method. Despite this advantage, GBM is not widely used outside Benguet. No earlier studies have documented that GBM can be implemented in an area using whole-ore amalgamation. Earlier technology transfer projects have promoted retorting of amalgam as a preventive technology in ASGM.

A project area in Mindanao, 20% of the miners have already converted to the mercury-free method.

Borax Method of Gold Extraction

Unfortunately, this method is ineffective in areas using whole-ore amalgamation, since up to 90% of the mercury is lost to the tailings (the waste product consisting of fine sand) and only 10% is lost by blowtorching of amalgam. Thus, only a small fraction of the mercury spill from whole-ore amalgamation can be recovered with a retort. The introduction of cyanidation techniques has also been suggested as a way to reduce or eliminate the use of mercury in ASGM. Although most cyanide compounds decompose into nontoxic forms, cyanide itself is highly toxic, and exchanging one toxic chemical with another may be regarded as a controversial solution.

BORAX RECOVERS MORE GOLD than MERCURY

 

Gold_recovery_using_amalgamation_vs._borax_smelting
Borax for Higher Gold Recovery

We present the results of a project in which GBM was introduced in two mining communities in the Philippines where whole-ore amalgamation was widely practiced. The main objective of the project was to reduce mercury pollution from small-scale gold mining by encouraging ASGMs to use a mercury-free method.

 

mercury_to_recover_gold
Nadine Steckling, Stephan Bose-O’Reilly, Dennis Shoko, Stefan Muschack, and Rudolf Schierl (2014) Testing Local Conditions for the Introduction of a Mercury-free Gold Extraction Method using Borax in Zimbabwe. Journal of Health and Pollution: October 2014, Vol. 4, No. 7, pp. 54-61.

Mercury Kills!

borax_method_to_recover_gold

This article aims to:

  1. describe the changes in mining practice in two ASGM communities after two years of project implementation.
  2. describe the activities undertaken to encourage the communities to adopt mercury-free gold mining using the borax method.
  3. explore enabling and hindering factors in phasing out mercury use.
  4. teach basic placer mining methods

Obtain the Full Story: Mercury Pollution from Small-Scale Gold Mining Can Be Stopped by Implementing the Gravity-Borax Method – A Two-Year Follow-Up Study from Two Mining Communities in the Philippines.

Mercury-Free Gravity-Borax Method Gold Recovery

Testing Local Conditions for the Introduction of a Mercury-free Gold Extraction Method using Borax in Zimbabwe

Special thanks to:

Rasmus Køster-Rasmussen, MD PhD
The Research Unit for General Practice
University of Copenhagen
Øster Farimagsgade 5
P. O. Box 2099
DK-1014 Copenhagen
Denmark

rakra@sund.ku.dk
www.fe.ku.dk

It is estimated that between 10 and 15 million artisanal and small-scale gold miners worldwide (most of which cannot afford quality mining equipment) include 4.5 million women and 600,000 children. According to UNIDO, as much as 95 percent of all mercury used in artisanal gold mining is released into the environment. UNIDO estimates that mercury amalgamation from this kind of gold mining results in the release of an estimated 1000 tons of mercury per year.

 

The U.S. Borax Boron Mine is the largest open-pit mine in California. It is probably the largest borate mining operation in the world. The pit is a mile long, half a mile wide and 500-feet deep. The company, a subsidiary of Rio Tinto, extracts several borate minerals from an ancient lakebed that had been buried by alluvium. Near Boron, San Bernardino Co., Calif.
California has the largest Borax Mine in the World and mines approximately three million tonnes of borate ore every year from the Boron mine. It produces nearly half of the world’s supply of refined borate products. The mine measures 2.8km wide, 3.2km long and is up to 230m deep. (Flickr)

Watch and Learn all about BORAX MINING USA

Further References:

  1. United Nations Industrial Development Organization (UNIDO). Protocols for Environmental and Health Assessment of Mercury Released by Artisanal and Small-Scale Gold Miners. 2004. (ISBN 92-1-106429-5). 2004. http://iwlearn.net/iw-projects/1223/reports/protocols-for-environmental-and-health-assessment-of-mercury-released-by-artisanal-and-small-scale-gold-miners/view
  2. Perez E, Appel PWU, Køster-Rasmussen R. Training of Small Scale Miners and their Families in Safe Handling of Mercury During Extraction of Gold in the Philippines. Improving Access to Social Services: health services and income opportunities for Small Scale Miners and Their Families.  Report for the World Bank from the Geological Survey of Denmark and Greenland (GEUS). 2007.  http://www.geus.dk/program-areas/common/geus_rep_2007-35.pdf
  3. The United Nations Environment Programme (UNEP). Technical Background Report for the Global Mercury Assessment 2013. http://www.amap.no/documents/doc/technical-background-report-for-the-global-mercury-assessment-2013/848
  4. Appel PWU and Na-Oy L. The Borax Method of Gold Extraction for Small-Scale Miners. Blacksmith Institute Journal of Health & Pollution. 2012. 2(3):5-10. http://www.journalhealthpollution.org/doi/pdf/10.5696/2156-9614-2.3.5
  5. Ministry of Foreign Affairs of Denmark (DANIDA). Policy for Danish Support to Civil Society. 2014.http://um.dk/en/~/media/UM/Danish-site/Documents/Danida/Samarbejde/Civil-org/Dokumenter/Strat/Civilsamfundspolitik_UK_web.pdf
  6. Ministry of Foreign Affairs of Denmark (DANIDA). The Right to a better life – Strategy for Denmark’s Development Cooperation. 2012. http://um.dk/en/~/media/UM/English-site/Documents/Danida/Goals/Strategy/13287_DANIDA_strategiformidling_UK_web.pdf
  7. Rogers EM. Diffusion of innovations. Fifth edition. Free Press. 2003.
  8. Heinemann Media, Diálogos, and LO/FTF Council.
  9. [accessed March 2015] Rather rich and healthy than poor and poisoned – Gold extraction with borax for small scale miners. 2012.http://www.youtube.com/watch?v=X6Sawj0HyF0
  10. Kristensen AKB, Thomsen JF, and Mikkelsen S. A review of mercury exposure among artisanal small-scale gold miners in developing countries. Int Arch Occup Environ Health. 2013; DOI 10.1007/s00420-013-0902-9
  11. Smallwood CL, Lipscomb J, Swartout , et al. Toxicological review of boron and compounds.  Washington, DC. U.S. Environmental Protection Agency. 2004:1-88.
  12. European Food Safety Authority Panel on Food Additives and Nutrient Sources added to Food. Scientific opinion on the re-evaluation of boric acid (E 284) and sodium tetraborate (borax) (E 285) as food additives. EFSA Journal. 2013;11(10):3407.
  13. European Chemicals Agency. [accessed March 2015] EU candidate list of substances of very high concern. http://echa.europa.eu/candidate-list-table
  14. Scialli AR, Bonde JP Brüske-Hohlfeld I, Culver BD, Li Y, and Sullivan FM. An overview of male reproductive studies of boron with an emphasis on studies of highly exposed Chinese workers. Reproductive Toxicology. 2010;29:10-24
  15. http://www.journalhealthpollution.org/doi/pdf/10.5696/2156-9614-2.3.5
  16. Mercury pollution from artisanal gold mining

Alternative to Mercury – GOLD MINING EQUIPMENT without Hg

alternative to mercury in gold mining

Click these mercury-free gold extraction machines images to learn more.
recover gold without mercury

Also see UNEP.