Merrill Crowe Flowsheet

Here is a common and classic merrill crowe process flowsheet with a simple zinc precipitation chemistry. Some of the flows in this design:

  1. Too much dilution water is used
  2. Zinc dust is added after the pump
  3. No mechanical seal is present on the pump to prevent O2 entry.

Merrill Crowe Flowsheet

 

Learn more about the Merrill Crowe Flowsheet.