Fire Assay Procedure

fire assay equipment (17)

Fire assaying has been practiced since ancient times and has proven to be very reliable in the determination of precious metals. References to fire assaying are found in the old testament of the Bible and artifacts in past civilizations’ ruins. Assaying began to appear in French and English literature in the 12th century and from […]

Gold Bullion Assay Procedure

Amount of Gold

The procedure for assay of gold bullion, as described has for its sole object the estimation of the percentage of gold present in the alloy, all other constituents being disregarded. In the first instance, the simple case of the assay of gold alloys containing appreciable quantities of only copper and silver will be dealt with. Refined […]

Parting the Assay Buttons

cupellation-tray

The assay buttons are flattened by a hammer weighing about 7 lbs., with a convex face, on an anvil kept quite bright and clean and used for this purpose only. A heavy blow is first delivered on the centre of the button, the diameter of which is thereby increased to nearly that of a threepenny […]

Weighing Gold for Assay Checks & Proofs

weighing_the_cornets_in_fire_assay

The balance must readily indicate differences of 0.005 per 1,000, or 1/40 milligramme, with a weight of ½ gramme in each pan. The “checks” or “proofs” (vide infra) are weighed first, and their mean excess or deficiency in weight applied as a correction to all the cornets worked with them. This may be done by means […]

How to Make Gold

Glass Tube

The purest gold obtainable is required for use as standards or check pieces in the assay of gold bullion. The following method of preparing it is now in use at the Mint. Gold assay cornets from the purest gold which can be obtained are dissolved in nitrohydrochloric acid, and the excess of nitric acid expelled […]

Fire Assaying Gold Alloys

fire-assay-gold-alloys

It is often impracticable to apply the ordinary parting assay to the examination of low-standard alloys of gold with other metals. These are then tested by various other methods, of which a summary is given below, the alloys being grouped in four series for convenience: A. Alloys requiring scorification. B. Amalgams. C. Alloys containing members […]

Bone Ash Cupels

bone-ash-cupels

In order to get a preliminary view of the question of gold absorption in cupelling gold bullion, certain samples of very pure gold, which were being sent out to various laboratories in the Mint service for comparative assaying, mere assayed in sets of sis with three proofs. The nine ctipe!i were arranged in the muffle […]

Cupellation

cupellation

A coke Cupellation furnace still in use at the Mint is shown in front and side elevation in Figs. 95 and 96. It consists of an outer casing of wrought-iron plates about 1/8 inch thick, united by angle iron. This casing is connected with a chimney 60 feet high by means of a wrought-iron hood, a, […]

Gold Fire Assay Process

fire assay equipment (13)

The Gold Fire Assay Process of ores is almost universally conducted in the dry procedure by furnace methods. Exceptions will be noted later. The plan of operation is to concentrate the precious metal in a button of lead either (1) Fire Assay By fusion in a crucible; or, more rarely, (2) Fire Assay By scorification. […]

Roasting Arsenic & Antimony Ores

Roasting Arsenic & Antimony Ores - 911Metallurgist

The difficulty of roasting arsenical and antimonial ores may be avoided by taking ore, 1 A.T. ; red lead, 1,000 grains; sodium carbonate, 500 grains; potassium ferrocyanide, 550 grains, with a cover of salt or borax. The button is scorified, together with the matte formed, before cupellation. E. A. Smith found this method unsatisfactory and […]