Table of Bond Work Index by Minerals

This Table of Ball Mill Bond Work Index of Minerals is a summary as tested on ‘around the world sample’.  You can find the SG of each mineral samples on the other table.

[table id=2 /]

Source 1: Table of materials reported by Fred Bond
Source 2: Outokumpu, The science of comminution
Source 3: Equipment and pipelines
Source 4: Tenova Bateman mills (AG/SAG, Rod, Ball Mill)
Source 5: Doering international GmbH www.cylpebs.com
Source 6: SME handbook of mineral processing, N.L Weiss Editor, NY 1985