If you are looking for an affordable Hydrocyclone Manufacturers, contact us.
Hydrocyclone is a continuous device that utilizes centrifugal force to accelerate the settling rate of particles. When feed slurry enters the hydrocyclone tangentially under pressure, as result of the high centrifugal forces, particles coarser than the “cut point” size migrate into a primary vortex adjacent to the wall and move forward to discharge with a small volume of water via the spigot. Particles finer than the “cut point” size migrate into a secondary upward-moving vortex, along the axis of the hydrocyclone and discharge with the majority of the water via vortex finder.
The Hydrocyclone is one of the most common classification unit in the minerals industry, it is widely used in the mineral industry processing as a classifier, which has proved extremely efficient at fine separation size. Hydrocyclone is widely used in closed circuit grinding operations but it also has many other applications, such as desliming, degritting, and thickening.
Features & Benefits
Compact and simple structure
No moving parts
Low investment and running cost
Easy to install and simple to operate
High efficiency
High erosion resistance
Technical Specification of out Hydrocyclone Manufacturer
Model
Interior Dia (mm)
Cone Angle
Overall Pipe Dia (mm)
Feeding Size (mm)
Feeding Pressure (Mpa)
Processing
Capacity
(m3/h)
Range
(um)
Dimensions
(L*W*H)(mm)
FX660
660
20
180-240
16
0.03-0.2
250-350
74-220
1250
890
2650
FX500
500
20
130-200
10
0.03-0.3
140-220
74-200
850
790
2050
15
74-150
850
790
2380
FX350
350
20
80-120
6
0.04-0.3
60-100
50-150
775
605
1765
15
50-120
775
605
2115
FX300
300
20
65-115
5
0.04-0.3
45-85
50-150
665
585
1310
15
40-100
665
585
1505
FX250
250
20
60-100
3
0.06-0.35
40-60
40-100
540
480
1180
15
40-100
540
480
1220
10
30-100
540
480
1380
FX200
200
20
40-65
2
0.06-0.35
25-40
40-100
435
360
1050
15
30-100
435
360
1115
10
30-100
435
360
1205
FX150
150
20
30-45
1.5
0.06-0.35
11-20
30-74
280
295
690
15
30-74
280
295
900
8
30-74
280
295
1270
FX125
125
17
25-40
1
0.06-0.35
8-15
20-100
210
185
620
8
20-74
250
240
985
FX100
100
20
20-40
1
0.06-0.35
5-12
20-100
260
210
525
15
20-100
268
215
720
8
20-100
268
215
1000
FX75
75
15
15-22
1.5
0.1-0.4
2-5
20-74
240
230
465
6
5-40
240
230
800
FX50
50
15
11-16
0.3
0.1-0.4
1-2
10-74
160
155
350
6
5-30
160
155
590
Copyright 2012-2024 911Metallurgist | All Rights Reserved