BOND WORK INDEX TEST BALL MILL

The FC Bond Work Index Test Ball Mill was designed by F. C. Bond for use in determining the Bond Index, a measure of grindability and power required for grinding applications. The FC Bond Mills are used in laboratories throughout the world. A copy of Fred C. Bond’s Method of Crushing and Grinding for determination of the Bond Index is included with each mill. This mill can be used to calculate the grindability of all ores.  width=This Ball Mill can be used in to grind for a period of time, if plugged into a lab timer, or it can be used for any number of revolutions, according to the type of grind desired. The FC Bond ball Mill comes with table stand (pictured), motor, clutch, revolution counter, motor starter* and controls, 12″ machined steel drum, 44-1/2 pounds of steel balls (Bond Index test), receiving pan and hand screen pan. Our Bond mill is guaranteed to have internal mill dimensions within 0.10” of the 12” x 12” as specified by Mr. Bond. This is important, because the original bond mill was within these specifications and all data derived by Fred Bond was derived from a mill with his specifications

bond_test_mill

Bond Ball Mill Work Index (Grindability Tests)

DESCRIPTION

All material used was Mild Steel – 1018 TOLERANCES HELD BELOW:

  • Shafts after weld .00005” on diameter (total – 1.4370 to 1.4375 dia.) tight slip fit bearing. Key way shaft .002 on diameter/width and .004 centerline. * Shafts threaded and screwed into end caps prior to weld and machined to size after weld.
  • Tube OD- Stock Diameter ID was stock at 12.030” diameter. End caps to match tube OD within .10” and threaded to match shafts. End caps were made with a light press fit into body (tube).
  • Inside 12” dimension from end cap to cap- held within .100” on average.
  • Mounting plate was a match fit to OD of radius to tube prior to weld.
  • Doors were a match fit to tube so door radius and ID of tube radius matched each other within .015” after gasket was installed.
  • After weld, all parts were checked for concentricity using Standard Pillow Block bushings – all parts ran within .005” when checked with indicator – this is worst case –most check with .003”.
  • All parts are deburred and lightly sanded after weld.
  • Welded shafts to endcaps- to support bushing to end cap to end cap to barrel mounting plate fused inside of end caps and mounting plate welded “T” nut assembly.