Designs for Small Portable and Mobile Gold Leaching Plant

small gold leaching equipmentportable gold cyanide leaching plant

 

mobile gold leaching plantcyanide leaching gold recovery process

 

extraction of gold from ore using cyanide
Secondary Crusher is recommended for efficient crushing in the 250 to 265 ton/day

Agitation capacity based on 36 to 48 hours of agitation time. Thickener area based on 6 to 7 square feet per ton of dry solids per 24 hours. Pregnant cyanide solution (Primary Thickener Overflow) is treated in a Precipitation System which includes: Clarifier, Vacuum Tank, Vacuum Pump, Clarifier Pump, Zinc Dust Feeder, Zinc Mixing Tank with Pump, and Precipitation Tank, Motors and Drives are included with all pumps and the Zinc Dust Feeder.