Pulp and Bullion Balances and Scales

Pulp and Bullion Balances and Scales

BALANCE, Pulp—For weighing ore, bullion and pulp samples, etc., for analysis. Rigidly constructed. Brass beam. Beam release of standard eccentric type. Gold plated steel knife edges and agate planes. Removable, nickel plated brass pans. Mounted on polished mahogany box with drawer which will accommodate the balance mechanism. With level and leveling screws.

BALANCE, Pulp—For weighing ore, bullion and pulp samples, etc., for analysis. Similar to No. 12131, but enclosed in polished mahogany and glass case, with counterpoised front sliding door, with drawer. Capacity, 150 grams or 5 Troy ounces; sensitiveness, 2 mg. or .03 grains; diameter of pans, 3 inches.

BALANCE, Hand

BALANCE, Hand—With set of troy weights down to % grain. Pans suspended chains. In metal box.

BALANCE, Portable Gold—A new, compact and convenient portable gold balance, self-contained, mounted in hardwood case. Capacity, 2 oz.; sensitiveness, % grain. When closed the parts do not shift regardless of how handled, and the balance is set up ready for use as soon as the case is opened. Dimensions, closed: 9x7x2/4 inches. Complete with set of weights from 1 grain to 1 oz. Troy, and brass forceps. Weights from 1 grain to 12 grains are of aluminum, from 1 pwt. to 1 oz. of brass

BALANCE, Hand—With horn pans suspended silk cords. Polished beam. In pasteboard box.
Without weights.
Length of beam, mm. ……………………………………………………… 150   190
Diameter of pans, mm. ……………………………………………………  60     80

BALANCE, Bullion

BALANCE, Bullion—Capacity, 20 kg. Sensitiveness, 1 gram. Provided with two weighing beams and sliding weights. One of these is graduated into 100 grams by 1 gram divisions. The other is graduated into 1000 grams by 100 gram divisions. A sliding weight on an extra bar permits quick balancing of the weighing container.

BALANCE, Bullion—Capacity, 2400 ounces Troy. Weighs 25 ounces on the beam hy % ounces.
With brass weights and counterpoise.
Size of platform, 10×14 inches.