Mining Methods VS Underground Crusher Location

underground crusher

In Section 2 we dismissed those “big-room” applications not needing fundamentally new equipment, and lumped all the rest together. Now, as we examine specific mine types, it is appropriate to differentiate within these categories the manner in which portable crushers might be used, and the consequent effect on desired machine parameters. The common yardstick by […]

Portable Rock Crushers

As it relates to portable crushers, the basic portability concept under investigation here might better be described by the phrase ”decentralized crushing to allow automated ore haulage”. Clearly this means more and smaller crushers exhibiting some degree of mobility, and automated ore haulage usually means belt conveyors. The trade-off is a necessarily more costly crushing […]

Conveyor Belt Calculating Chart

The accompanying chart has been drawn for the convenience of engineers as a means of quickly determining the correct number of plies of conveyor belts operating under specific conditions. The calculations are based on the average safe strength (factor of safety, 15) of the various standard rubber conveyor belts. The calculations assume maximum loading conditions; […]

Stamp Mill Cam

The cams at present universally used in stamp mills lift the tappets with an involute form of curve, to which the surface of the tappet is always tangent; moreover, the line of contact between tappet and cam, if produced, would pass through the center of the stem. This is no doubt a desirable feature, but […]

Grinding Mill Design & Ball Mill Manufacturer

motion inside a rod mill

All Grinding Mill & Ball Mill Manufacturers understand the object of the grinding process is a mechanical reduction in size of crushable material. Grinding can be undertaken in many ways. The most common way for high capacity industrial purposes is to use a tumbling charge of grinding media in a rotating cylinder or drum. The […]

Cone Crusher Parts

cone crusher parts

Cone Crusher SPIDER CAP The cast steel spider cap has been designed to serve as a feed distribution plate for coarse materials. It is recessed on the 22, 30, 36 and 48-in. crushers. For fine materials, the wobble plate feeder — a more effective means of distributing the feed — is recommended. TOP SHELL AND […]

Difference between Crushing and Grinding

When making comparisons of the efficiencies of different grinding and crushing machines it is desirable to be able to estimate the work actually done in crushing the ore from a given size of feed to a given size of product, the screen analysis of both feed and product being determined. Messrs. Klug and Taylor, in […]

Sieve Analysis Calculations and Graph

The experiments described in this paper were undertaken primarily for the purpose of measuring the quality of work done in screening and sorting in American concentrating-mills for Prof. Richards’ work on Ore-Dressing. For this purpose a series of samples of screened and sorted products was obtained from four different mills, and a plan was devised […]

Silver Lead Ore Processing by Roll Crushing & Jigging

The following brief paper is intended, to apply to the concentration of the silver-lead ores at Broken Hill, New South Wales, generally, but more particularly to the process as applied to the ores in the Block 10 mine. The attached plans are similar in many respects to those prepared recently for the Block 10 Company. […]