Regrind Ball Mill Design Calculations 
                           
          Model Input     Model Output        
  Feed F80 (μm)     Total work required to P80 (kwh/short ton)
  Product P80 (μm)     Total kW to P80  (raw-unajusted)  
  Work index Kwh/short ton     Total HP to P80 (raw-unajusted)  
  Reduction ration if < 6 then -> EF2 (Table VIII)      
  Feed rate to regrind mill MTPH     EF5        
  Feed rate to regrind mill STPH     EF7 (Common of Regrinds)    
  Suggested L/D Ratio (Table VI) 1.75-2.0                
          D (m) (Table VII) (inside liners)  
              L (m) (Table VII)      
          Ball Size (mm) (Table VII)    
                40 % Ball Charge (Table VII)    
                Power (HP) (Table VII)    
                SS, HP ?      
                Ball Charge (MT) (Table VII)    
                HP Loss for small balls    
              Power, HP (calc from Table VII data)  
                Power, HP (calc from efficiency factors)  
                L Updated (m) (Table VII)    
                         
                           
                           